Assessment of the high-temperature crack behavior for a 316L stainless steel structure with defects
Hyeong-Yeon Lee/ Gyeong-Hoi Koo/Jae-Han Lee
The Journal of Mechanical Science and Technology, vol. 24, no. 2, pp.481-487, 2010
Abstract : An assessment of creep-fatigue crack initiation and growth for a 316L stainless steel structure has been carried out according to the
current (2007 edition) and previous (2002 edition) versions of the French RCC-MR A16 procedure. Some significant changes have been
made in terms of the formulae and material properties, which may cause big differences in the assessment. In this study, the changes in
the A16 guide have been quantified for a 316L austenitic stainless steel structure, and the assessment results were compared with those of
the observed images from a structural test for a welded component.
Keyword : Creep-fatigue; Crack initiation; Crack growth; 316L stainless steel; Defect |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
JMST Editorial Office: #702 KSTC New Bldg, 22 7-gil, Teheran-ro, Gangnam-gu, Seoul 06130, Korea
TEL: +82-2-501-3605, E-mail: editorial@j-mst.org |
JMST Production Office: #702 KSTC New Bldg, 22 7-gil, Teheran-ro, Gangnam-gu, Seoul 06130, Korea
TEL: +82-2-501-6056, FAX: +82-2-501-3649, E-mail: editorial@j-mst.org |
|
|
|
|